To study the effect of different scratch depths on the formation of scratches, combined with the experimental data in the process of magnetorheological polishing, the simulated scratch depths were selected to be 1.5, 2.0, and 2.5 nm. The GaAs material is selected as the (100) crystal plane, and the abrasive grain size is 8 nm.