Currently, the most common way to sinter SrTiO3 is using traditional high temperature methods, with the base material requiring temperatures > 1400 C to densify to >95% of theoretical.21 Whilst effective, this type of high temperature processing has a number of inherent drawbacks such as high energy costs and sometimes uncontrolled grain growth, meaning that any potentially desirable nanostructures (e.g. for the control of thermal conductivity in thermoelectric materials)22 are lost.
0/5000
源语言: -
目标语言: -
结果 (简体中文) 1: [复制]
复制成功!
目前,为了烧结钛酸锶是使用传统的高温方法中,与需要的温度> 1400的基体材料的最常见的方式是什么?C至致密化到的theoretical.21虽然有效> 95%,这种类型的高温处理的具有许多固有缺点,例如高的能源成本和有时不受控制的晶粒生长,这意味着任何潜在期望的纳米结构(例如在热电材料的热导率的控制)22都将丢失。
正在翻译中..
结果 (简体中文) 2:[复制]
复制成功!
目前,烧结 SrTiO3 的最常见方法是使用传统的高温方法,基础材料需要温度 = 1400 C 才能使理论密度达到 ±95%。固有的缺点,如高能源成本,有时不受控制的谷物生长,这意味着任何潜在的理想的纳米结构(例如控制热电材料的导热性)都丢失了。
正在翻译中..
结果 (简体中文) 3:[复制]
复制成功!
目前,烧结SrTiO3最常用的方法是使用传统的高温方法,需要温度>1400  C的基材才能致密到理论值的95%以上。21虽然这种高温处理有效,但它有一些固有的缺点,如能源成本高,有时晶粒生长不受控制,这意味着任何潜在的理想纳米结构(例如,用于控制热电材料中的热导率)22都将丢失。
正在翻译中..
 
其它语言
本翻译工具支持: 世界语, 丹麦语, 乌克兰语, 乌兹别克语, 乌尔都语, 亚美尼亚语, 伊博语, 俄语, 保加利亚语, 信德语, 修纳语, 僧伽罗语, 克林贡语, 克罗地亚语, 冰岛语, 加利西亚语, 加泰罗尼亚语, 匈牙利语, 南非祖鲁语, 南非科萨语, 卡纳达语, 卢旺达语, 卢森堡语, 印地语, 印尼巽他语, 印尼爪哇语, 印尼语, 古吉拉特语, 吉尔吉斯语, 哈萨克语, 土库曼语, 土耳其语, 塔吉克语, 塞尔维亚语, 塞索托语, 夏威夷语, 奥利亚语, 威尔士语, 孟加拉语, 宿务语, 尼泊尔语, 巴斯克语, 布尔语(南非荷兰语), 希伯来语, 希腊语, 库尔德语, 弗里西语, 德语, 意大利语, 意第绪语, 拉丁语, 拉脱维亚语, 挪威语, 捷克语, 斯洛伐克语, 斯洛文尼亚语, 斯瓦希里语, 旁遮普语, 日语, 普什图语, 格鲁吉亚语, 毛利语, 法语, 波兰语, 波斯尼亚语, 波斯语, 泰卢固语, 泰米尔语, 泰语, 海地克里奥尔语, 爱尔兰语, 爱沙尼亚语, 瑞典语, 白俄罗斯语, 科西嘉语, 立陶宛语, 简体中文, 索马里语, 繁体中文, 约鲁巴语, 维吾尔语, 缅甸语, 罗马尼亚语, 老挝语, 自动识别, 芬兰语, 苏格兰盖尔语, 苗语, 英语, 荷兰语, 菲律宾语, 萨摩亚语, 葡萄牙语, 蒙古语, 西班牙语, 豪萨语, 越南语, 阿塞拜疆语, 阿姆哈拉语, 阿尔巴尼亚语, 阿拉伯语, 鞑靼语, 韩语, 马其顿语, 马尔加什语, 马拉地语, 马拉雅拉姆语, 马来语, 马耳他语, 高棉语, 齐切瓦语, 等语言的翻译.

Copyright ©2024 I Love Translation. All reserved.

E-mail: