The advantages of CSP over other sintering processes can be summarized [25–29]:(i) Ultra-low sintering temperature(300°C) due to facilitated mass transport kinetics by mechanical-chemical couplings. (ii) Capability to fabricate nanostructured ceramics due to ultra-low sintering temperature and short duration.