In Example 3, graphene-coated PAN fibers were compacted and melted together to form several composite films, which were subjected to the following heat treatments: 250°C for 1 hour, 350°C for 2 hours, and 1000°C. for 2 hours to obtain the graphene-carbon foam layer.