对钢管预热温度不易达到温度要求及温度降低快的现象,在喷砂除锈完成后,设专人提前用烤把对管子表面持续均匀加热,当防腐工进行该焊口的防腐补口作业的英语翻译

对钢管预热温度不易达到温度要求及温度降低快的现象,在喷砂除锈完成后,设

对钢管预热温度不易达到温度要求及温度降低快的现象,在喷砂除锈完成后,设专人提前用烤把对管子表面持续均匀加热,当防腐工进行该焊口的防腐补口作业时,再移到下一道口提前进行预热。为了抵消低温环境下的热量散失效应,在对焊口预热时,应达到预热温度要求的上限,温度控制采用红外测温仪测量,沿圆周均测8点
0/5000
源语言: -
目标语言: -
结果 (英语) 1: [复制]
复制成功!
The preheating temperature of the steel pipe is not easy to meet the temperature requirements and the temperature drops quickly. After the sandblasting and rust removal are completed, a special person shall be used to heat the surface of the pipe uniformly in advance with a roasting handle. , Then move to the next port for preheating in advance. In order to offset the failure of heat dissipation in low temperature environment, when the butt weld is preheated, the upper limit of the preheating temperature should be reached. The temperature control is measured by an infrared thermometer, and 8 points are measured along the circumference.
正在翻译中..
结果 (英语) 2:[复制]
复制成功!
The warm-up temperature of the steel pipe is not easy to reach the temperature requirements and the phenomenon of rapid temperature reduction, after the completion of sand blasting rust removal, set up a special person in advance with a baking put to the pipe surface continuously and evenly heated, when the anti-corrosion worker to carry out the anti-corrosion filling operation of the weld, and then move to the next port to preheat in advance. In order to offset the heat dispersion failure in low temperature environment, when preheating the weld, the upper limit of the preheat temperature requirement should be reached, the temperature control is measured by infrared thermometer, and 8 points are measured along the circumference.
正在翻译中..
结果 (英语) 3:[复制]
复制成功!
For the phenomenon that the preheating temperature of the steel pipe is not easy to meet the temperature requirements and the temperature drops rapidly, a special person shall be assigned to heat the pipe surface continuously and evenly with the baking handle after the sand blasting and rust removal is completed. When the anti-corrosion workers carry out the anti-corrosion joint repair work of the welding joint, they will move to the next pass for preheating in advance. In order to counteract the heat loss effect in low temperature environment, the upper limit of preheating temperature should be reached when preheating the welding joint. The temperature control is measured by infrared thermometer, and 8 points are measured along the circumference<br>
正在翻译中..
 
其它语言
本翻译工具支持: 世界语, 丹麦语, 乌克兰语, 乌兹别克语, 乌尔都语, 亚美尼亚语, 伊博语, 俄语, 保加利亚语, 信德语, 修纳语, 僧伽罗语, 克林贡语, 克罗地亚语, 冰岛语, 加利西亚语, 加泰罗尼亚语, 匈牙利语, 南非祖鲁语, 南非科萨语, 卡纳达语, 卢旺达语, 卢森堡语, 印地语, 印尼巽他语, 印尼爪哇语, 印尼语, 古吉拉特语, 吉尔吉斯语, 哈萨克语, 土库曼语, 土耳其语, 塔吉克语, 塞尔维亚语, 塞索托语, 夏威夷语, 奥利亚语, 威尔士语, 孟加拉语, 宿务语, 尼泊尔语, 巴斯克语, 布尔语(南非荷兰语), 希伯来语, 希腊语, 库尔德语, 弗里西语, 德语, 意大利语, 意第绪语, 拉丁语, 拉脱维亚语, 挪威语, 捷克语, 斯洛伐克语, 斯洛文尼亚语, 斯瓦希里语, 旁遮普语, 日语, 普什图语, 格鲁吉亚语, 毛利语, 法语, 波兰语, 波斯尼亚语, 波斯语, 泰卢固语, 泰米尔语, 泰语, 海地克里奥尔语, 爱尔兰语, 爱沙尼亚语, 瑞典语, 白俄罗斯语, 科西嘉语, 立陶宛语, 简体中文, 索马里语, 繁体中文, 约鲁巴语, 维吾尔语, 缅甸语, 罗马尼亚语, 老挝语, 自动识别, 芬兰语, 苏格兰盖尔语, 苗语, 英语, 荷兰语, 菲律宾语, 萨摩亚语, 葡萄牙语, 蒙古语, 西班牙语, 豪萨语, 越南语, 阿塞拜疆语, 阿姆哈拉语, 阿尔巴尼亚语, 阿拉伯语, 鞑靼语, 韩语, 马其顿语, 马尔加什语, 马拉地语, 马拉雅拉姆语, 马来语, 马耳他语, 高棉语, 齐切瓦语, 等语言的翻译.

Copyright ©2024 I Love Translation. All reserved.

E-mail: