The applied temperature is, however, high enough to melt the SrCl2 phase, and it is likely that this also aids flow of particles around one another during pressing. The temperature is not high enough to cause any significant reaction of the SrCl2 and TiO2 phases, and both are observable as crystalline by XRD after CS (Fig. 1c).