For this estimation, dissolution–precipitation was assumed to occur predominantly between the vaterite agglomerates, as suggested by the necks formed between them in the SEM images shown in Fig. 3a (inset). By contrast, attempts to fit the creep data of nanovaterite specimens pressed at 40 MPa and above led to an overestimation of the strain rate by several orders of magnitude (see Supplementary Fig. 6).