When a similar program evaluated the repair of a much higher strength 7050-T6 substrate, the performance of the cold spray material mechanical properties in comparison to the substrate were not the preferred situation of higher cold spray material mechanical properties. This is due in large part to the 7050 wrought alloy gaining so much strength from heat treatment that the cold sprayed material cannot achieve the same ultimate and yield strength, see Table 2.