Fig. 3 shows an SEM image of cold sintered MnO where two distinct grain size populations are evident. The larger population with;2um average diameter corresponds to the initial powder, while the much smaller population with 100 nm diameter, and are those which formed during cold sintering. This pellet was cold sintered at 250 °C under 300 MPa of pressure for 30 min. A