*Resistance to impact:Tests shall be carried out at -30oC after conditioning the test objects for at least 4 hours at that temperature. At - 30oC no splinter is allowed and the part shall be fully functional after the impac t. No visible cracks shall appear after 1 ± 0.2 J impact with a 1000 g steel ball.