In another study, geopolymer-SiC components were produced by using geo-polymer as a binder. At the end of 30 min at 130℃ under a pressure of 240 MPa, depending on the initial precursor type, relative densities reaching to 90% (having around 170 MPa compressive strength) was able to be achieved [261].