WP has great similarity with HHP and CS in terms of procedure [260]. Usually, it is operated with the help of a solution (solution-precipitation assisting medium) at temperatures =300℃ under a constant uniaxial pressure (e.g. =240 MPa) to densify the products. The heat is conducted axially through pressing plates similar to the direction of the applied pressure which is different for CS and HHP.