After 12 hours of concrete pouring, pick up the floating slurry and loose concrete whose surface is about 10-20mm higher than the bottom surface of the slab and rinse them with water
After the concrete pouring is completed for 12h, the laitance and loose concrete with the surface 10-20mm higher than the bottom surface of the slab shall be chiseled out and washed with water<br>