Our rework program is as follows:<br>1, first of all, the four large holes in the illustration position to take laser cladding technology for welding, about one-sided thickening 0.5mm;<br>2, milling to go up and down the box parting side single side about 0.3mm;<br>3, the two sides after correction, mounted positioning pin, tight bolts, re-processing four large holes to the drawing requirements, while lighting out the two sides.