The straight cyanidation procedure is selected to recover the gold from the ore because of the simplicity and economy of the process. NaCN has the ability to leach the gold even at a very low concentration or strength of solution, ranging from 0.01 – 0.10 % CN strength.The leaching time required may vary from 16 – 72 hours, depending on the nature and characteristic of the gold.