The shear created from the rotating screw is generating heat and higher temperature than the set point and the barrel heaters are no longer being used to control the barrel temperature at all. If this is the case look at reducing the screw rotation speed to allow the screw to recover 2–3 seconds prior to mold open, or examine the back pressure being applied to the screw.