When FAEA is used alone, the delignification rate of wheat straw is 38%, and when FAEA is combined with xylanase and laccase, the delignification rate reaches 55%.
When FAEA was used alone, the delignification rate of wheat straw was 38%, while when FAEA was combined with xylanase and laccase, the delignification rate reached 55%
When FAEA was used alone, the delignification rate of wheat straw was 38%, while when FAEA was combined with xylanase and laccase, the delignification rate reached 55%.