Please se attached pictures. The customer has reported a rejection for porosity in the casting that has become visible once the part is welded into place. They are thinking that the parts look like they have been welded up and then hand ground back. Is this happening at the factory as a repair for poor castings? Please speak to the factory and advise on why this might be happening as we also had this issue last year.