The bed temperature can be controlled at the optimum reaction temperature by spraying water, the best gas-solid inter-turbulent turbulence mix ingestion and constantly exposing the new surface of unreacted lime, while the desulfurization agent has a long stay time through the multiple cycles of solid material, thus greatly improving the calcium utilization rate of the desulfurizer and the desulfurization efficiency of the reactor.