In the wavelength range of 380~1100nm, the surface of DWS mc-Si has prepared suede with a reflectivity of 25%, while the reflectivity of LASS mc-Si is 23%. Obviously, the results of the two are very close.
In the wavelength range of 380 to 1100 nm, the DWS mc-Si surface prepared a 25% fluctuating rate, while the LASS mc-Si had a reflectivity of 23%, and the results were clearly very close.
In the wavelength range of 380 ~ 1100nm, suede leather with reflectivity of 25% was prepared on DWS MC Si surface, while that of lassmc Si was 23%. It is obvious that the results of the two methods are very close