The top view and the bottom view of the final casting are shown in Fig. 14(a) and Fig. 14(b). Radiographic testwere performed on the final casting. The test confirmed that there exist no internal defects (shrinkage porosity) inthe casting. With manual inspection, it has been observed that the casting was free from surface defects. Hence itwas concluded that experimental results were confirmed with simulation results.