The used laser parameters are listed in Table 2. Moreover, the dimension of each laser transformation hardened region was 60 × 25 mm2 . After completing the first hardening process, the hardened region was placed till reaching the room temperature. Then, the second hardening process would be carried out at a gap of 30 mm (A total of five LTH processes were processed).