. Favorable bulk morphology and enhanced electronmobility were induced by slowing solvent evaporation rate.The resulting PTB7–Th/PNDIS-HD OSCs achieved a PCE as highas 7.7% with a Jsc of 18.8 mA cm2, which is about two foldsenhanced compared with the thermally (175 C) annealeddevice.