Our rework solutions are as follows:<br>1, first of all, the four large holes in the illustration position to take laser cladding technology for welding, about one-sided thickening 0.5mm;<br>2, milling on and off the box parting surface single-sided about 0.3mm;<br>3, the two sides after correction, mounted positioning pin, tight bolts, re-machining four large holes to the drawing requirements, while milling out the two sides.