3.5.1.1 Tensile Properties Shall be as specified in Table 2, determined in accordance with ASTM E 8 with the rate of strain set at 0.005 inch/inch/minute (0.005 mm/mm/minute) and maintained within a tolerance of ±0.002 inch/inch/minute (0.002 mm/mm/minute) through the 0.2% offset yield strain. 3.5.1.1.1 Tensile property requirements apply in both the longitudinal and transverse directions. Transverse tensile properties of Table 2 apply only to product that a test specimen not less than 2.50 inch (63.5 mm) in length can be obtained.