1.3.3 Working electrode preparation<br>MnO2/PPy (or MnO2), acetylene black, binder (PVDF) mixed evenly in a quality score of 7:2:1, coated on a 1 cm2 foam nickel set fluid, dried 4 h in a drying chamber at 75 degrees C, pressed tablets, made working electrodes, stored in self-sealed bags, spare.