SEM images of the green pellets and specimens sintered at different temperatures for 4 h are shown in Fig. 5. The green pellets seemed to be quite dense but possessed chunks of agglomerated particles, as shown in Fig. 5(a). The samples still possessed these agglomerated particles after sintering at 400°C (Fig. 5(b)).