In Example 3, graphene coated PAN fibers are compacted and melted together to form several composite films, which are subjected to the following heat treatments: 1 hour at 250 ° C, 2 hours at 350 ° C, and 2 hours at 1000 ° C to obtain graphene carbon bubbles<br>Foam layer.