The εr values initially increased from 15.51 to 15.65 at a temperature range 800°C–850°C, with a maximum of 15.68 observed at 900°C and then decreased slightly at a temperature above 900°C. A similar trend was also observed in the apparent density, which proved that the density played a dominant role in determining the dielectric permittivity of samples with a fixed phase composition [33].