Our rework solutions are as follows:<br>1, the first step, four large holes in the illustration position to take laser cladding technology for welding, about one side thickened 0.5mm, according to our past.<br> With processing experience, this welding produces little deformation to the part itself.<br>2, the second step, milling up and down the box parting surface, one side about 0.3mm thickness;<br>3, finally, the two sides of the box body correction in place, loaded with positioning pins, tight bolts, re-machining four large holes to the drawing requirements, while milling the two sides of the box assembly plane.