In the range of 170-270℃, the weight loss of [EMIM] PF6-D301 resin is significantly higher than that of D301 resin, indicating that [EMIM] PF6 begins to decompose around 170.
In the range of 170-270 degrees C, the weight loss of the PF6-D301 resin is significantly higher than that of the D301 resin, indicating that the PF6 begins to decompose around 170.
In the range of 170-270 ℃, the weight loss of [EMIM] pf6-d301 resin was significantly higher than that of D301 resin, indicating that [EMIM] PF6 began to decompose around 170,<br>