It can be seen from Figure 8 that under different drying conditions, all powder samples have abundant nanopores (≤300 nm), especially pores less than 50 nm.
It can be seen from Fig. 8 that all powder samples have abundant nano pores (≤ 300 nm), especially pores less than 50 nm under different drying conditions.