A certain amount of nanosilver wire suspension was evenly dropped on the surface of the glass substrate, then the spin coating speed was increased to 500 rpm/s at an acceleration of 50 rpm/s, spin coating was performed for 5 s, and then the coating was applied at an acceleration of 50 rpm/s. Increase the spin coating speed to 2000 rpm/s and spin coating for 10 s. Remove the sample and heat treat it under an infrared lamp for 5 minutes.