The hot zone designated prior to the pipe rupture was not of sufficient size to ensure that individuals outside of the hot zone were safe from the hightemperature, flammable 4-sidecut process fluid when the sulfidation failure of the pipe occurred. As discussed in subsequent sections of this report, it is beneficial for various personnel with differing areas of process expertise to report their knowledge of the leak properties and potential causes of the leak to the Incident Commander.