Similar dielectric behavior, i.e. broad peak at the Curie temperature and relatively low dielectric constant was very recently reported for cold sintered BaTiO3 ceramics obtained at 300oC and explained mainly in terms of grain size effects [32]. Together with this recent report, the data in the current work supports that it is possible to obtain decent dielectric properties even by sintering at low processing temperatures via rHLPD.