As specified for the parent metal in the transverse direction, but at least 27 J3). By way of derogation from this, if ferritic-austenitic, austenitic and nickel base-alloy filler metals are used: 40 J3). The test is carried out at the lowest working temperature, but not lower than the test temperature in the parent metal test and not higher than 20 °C