When required (see ordering information), the effective case depth shall be as specified. It shall be the as nitrided case depth at which the values specified in Table 4, converted from microindentation hardness, are obtained by performing a hardness traverse in accordance with ASTM E384. In cases where the engineering drawing or purchase order specifies post nitride surface removal (see Ordering Information), the reported effective case depth shall include the amount to be removed.