connection preventing RFI, distortion and signal loss.
How Does DeoxIT® Gold Actually Work?
Conduction through a DeoxIT® Gold coated surface
takes place in three ways. First, DeoxIT® Gold can be
displaced by electrical arc, shock wave or simple
mechanical pressure and will redistribute itself along the
surface when the disturbance is removed. Second, a thin
insulating film of DeoxIT® Gold can be dispersed by an
electrical field. Finally, conduction takes place through
very thin films of DeoxIT® Gold by means of a quantum-mechanical phenomenon called “tunneling.”
To avoid detouring into a discussion in physics, simply
stated, electrons travel from one side of a thin film of
DeoxIT® Gold to the other without passing through (this
is the same effect that gave the tunnel diode its name).
DeoxIT® Gold fills the gaps in the contact surfaces,
increasing the surface area and current flow (conductivity). DeoxIT® Gold penetrates the plated surface and
molecularly bonds to the base metal to seal and protect
it (see FIGURE 1). Unlike other products, DeoxIT® Gold
provides long-lasting protection and will not gum-up,
evaporate, varnish, char or breakdown.
Virtually Unlimited Uses for DeoxIT® Gold
DeoxIT® Gold is ideal for use on Gold, precious metal
surfaces, plated contacts and connectors, edge connectors, IC's & sockets, connectors, contacts, plugs
& sockets, relays, circuit
boards (for storage),
s t a t i o n a r y / m o v i n g
connections, and
similar/dissimilar metals.
Use DeoxIT® Gold to
improve and maintain
the performance &
reliability of all electrical
components & equipment.
MANUFACTURER DISCLAIMER:
To the best of our knowledge, the information contained
herein is accurate. However, neither CAIG Laboratories, Inc.,
or any of its subsidiaries assumes any liability whatsoever for
the accuracy or completeness of the information contained
herein. All materials may present unknown hazards and
should be used with caution. In particular, improper use of
our products and their inappropriate combination with
other products and substances may produce harmful results
which cannot be anticipated. Final determination of the
suitability of any material is the sole responsibility of the user.
Although certain hazards are described herein, we cannot
guarantee that these are the only hazards that may exist. All
service performed on internal parts and equipment should
be provided by qualified technicians.
FIGURE 8. Shown - Dendrite corrosion
caused by excessive use of a circuit cooler.
Plated Surface
Base Metal
Deoxidized Contact Area.
Clean & Deoxidized Surface
is then Protected by a DeoxIT7 Gold Micro-Thin Layer