Notably, only the relative intensity of different components changes increasing the oxidation temperature from 427 to 600 C. Finally, the severe re-oxidation at 900 C for 5 h results in the formation of stable species (e.g. Ni-aluminate spinel species), formed by diffusion of NiOx into the Al2O3. These species are difficult to be reduced.1