Obviously, some of the larger agglomerated particles were broken into smaller particles after sintering at 500°C,as indicated by the yellow arrows in Fig. 5(c), and the microstructure appeared to be slightly loosened. Very few larger agglomerated particles remained, with small agglomerated particles possessing a more uniform size of ~60 nm after sintering at 600°C (Fig. 5(d)).