The improved experimental procedure, the Ba0.68Sr0.32TiO3 precursor was used to replace terpineol. The sample covered with polyimide sheets was pretreated under different pressure, duration, and temperature conditions with a flat vulcaniser. After pretreatment, the samples were sintered at 875–950 °C for 30 min.