Flexural Test. Similarly, 6 samples of pure epoxy and BFCP were prepared in the dimension of, 12.7 mm width, 6 mm in thickness and 127 mm in length. The specimens were tested under ASTM D790-03 [16]. UTM was used to carry out the three-point bending test with the strain rate of 5 mm/min.