slight increase in hole concentration with increasing f could be ascribed to interfacial defects,25 such as dangling bonds and anti-site defects, and the increase in hole concentration for the composite samples (f 0.3wt.%) probably because more interfacial defects are formed with increasing GaAs content, however, as f increasing further hole concentration decreases due to the agglomeration of the GaAs particles.