The mixed cement slurry is molded in PVC tubes with diameters of 10 mm and heights of 30-35 mm, and 24 hours later the cylindrical test pieces are removed for maintenance in the standard maintenance chamber for 28 days, and then drying and absorbent tests are carried out, and the detailed experimental process is shown in Figure 1.