In addition, we control the total doping amount to be constant and change the relative ratio of silicon oxide and aluminum oxide. The purpose is to find a better mixing ratio to maximize the performance of antigen oxygen.
In addition, we control the constant total doping volume and change the relative ratio of silicon oxide and alumina in order to find a better mixing ratio for optimal anti-atomic oxygen performance.