Predisperse phase (1) in order to obtain a homogeneous product at 70-75ºC2. Heat phase (0) 70-75ºC3. Emulsify phase (0) in phase (1) with high shear mixer 10 minutes. After cool with gentle stirrer4. Add remainig ingredients in main bulk at T< 38ºC5. Apply high shear mixer within 5 minutes in order to obtain the final viscosityCONTROL