Added Case Hardening specification on surfaces after finishing and shot peening.Surface hardness on sealings and bearings seat after finishing (NOT VALID for needle bearings)(1) Scales and types of hardness as per Table 4.(2) Can exceed by 1 HRC over the Max. drawingThe hardness test methods and the scales to be used depend on the CmtE/CHD values required as shown in Table4.