Elastomer and rubber parts are aged at a temperature of (100 2) °C for 70 h. After the test, the parts shall withstand the test of Clause D.2 using 75 % of the values indicated in Table D.1. For the test in accordance with Clause D.2, the parts may be tested individually or reassembled in the tool. If a part is tested reassembled in the tool, the test shall only be conducted between live parts and accessible parts.