Judging splices by micrographs, each single strand can be detected and all single wires are connected / welded at the outer surface. With Aluminium wires it’s sometimes hard to detect the single strands. There are still air locks / holes visible between the strands. The micrograph itself has just an informative character. Only if peel- and pull results in safe range a connection can be assessed as good.