In this experiment, when the mass ratio of aluminum oxide and silicon oxide reaches 1/3, the two kinds of particles form a more favorable form through the action of chemical bonds.
In this experiment, when the mass ratio of alumina to silica reaches 1 / 3, a more favorable morphology is formed by the chemical bond between the two particles.<br>